Polymer Property : Tensile Strength, Ultimate = 2190 psi
Polymer Property :
Tensile Strength, Ultimate =
2190 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength, Ultimate
11.7
-
15.1
MPa
1700
-
2190
psi
ASTM D638-95
Multibase Multi-Flex® TPO DEFA 1047
The burn rate is 0.53 in/min; ASTM FM VSS 302.Data provided by Multibase.