Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® TPO DEFA 1047

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Multibase
Trade Name Multi-Flex® TPO
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPO DEFA 1047.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The burn rate is 0.53 in/min; ASTM FM VSS 302.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.890 g/cc
0.0322 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955-89
Melt Flow 2.8 g/10 min
2.8 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 50
50
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 11.7 - 15.1 MPa
1700 - 2190 psi
ASTM D638-95
Elongation at Break 500 - 800 %
500 - 800 %
ASTM D638-95
Elongation at Yield >= 19 %
>= 19 %
ASTM D638-95
Flexural Modulus 0.0344 - 0.0482 GPa
4.99 - 6.99 ksi
Secant 1%; ASTM D-790-95
Izod Impact, Notched NB
NB
ASTM D-256-93a
Tear Strength Test 93 - 106
93 - 106
ASTM D624-95