Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 75.0 - 222 MPa
10900 - 32200 psi
Average value: 145 MPa Grade Count:80
Overview of materials for Nylon 610, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap..