Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 25.0 - 178 MPa @Temperature -40.0 - 150 °C |
3630 - 25800 psi @Temperature -40.0 - 302 °F |
Average value: 66.1 MPa Grade Count:9 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |