Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | ASTM D638-95 |
Multibase Multi-Pro® 1012 C BLK Medium Impact Mineral Filled Polypropylene Mineral filled PP compound for interior automotive applications. Product meets GMP PP 056 and EBG-M4 D605-A specifications. Ash is 10%.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PE-30MC-20TC/000 High Density Polyethylene (HDPE), Talc Filled
(discontinued **) Description/Features:Mica FilledTalc FilledInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 26.2 - 160 MPa | 3800 - 23200 psi | Average value: 121 MPa Grade Count:41 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | ASTM D638 |
American Polymers API 505 HF Polystyrene API 505 HF is a high flow, intermediate grade of impact modified polystyrene. This material possess exceptional moldability and easy colorability. API 505 HF offers good retention of mechanical pr.. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | ASTM D412/D638 |
Lubrizol STAT-RITE® X-5091 Ether-Type Static Dissipative Polymer Description: Inherently dissipative, this patented technology delivers surface resistivity in the range of 10E8 to 10E10 O/square. Stat-Rite® IDP Polymers forms a molecular-scale, interpenetrating .. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | ASTM D412 |
Lubrizol Estane® 2103-80PF Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film and profile resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in.. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | |
Cytec EN-2550 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | ASTM D638 |
DuPont™ Surlyn® 9020 Ionomer Resin, Zinc Surlyn® 9020 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The resin contains an addit.. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | ASTM D638 |
Devcon Brushable Ceramic - Red, Blue Epoxy Precision Repair EpoxyComments: Low-viscosity, alumina-filled, brushable epoxy compound, when applied to a 15-20 mil coating, provides a smooth, protective barrier against wear, abrasion, corrosion,.. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | ASTM D638 |
Devcon Brushable Ceramic - White Epoxy Precision Repair EpoxyComments: Low-viscosity, alumina-filled, brushable epoxy compound, when applied to a 15-20 mil coating, provides a smooth, protective barrier against wear, abrasion, corrosion,.. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | ASTM D638 |
Devcon Sprayable Ceramic™ Epoxy Precision Repair EpoxyComments: A sprayable ceramic-reinforced composite that can be sprayed in a manner similar to high-solid paints. Ideal for protecting pumps, paper machines, stacks, pump pads,.. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | Molded property |
Dow DOWLEX™ 2045 Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2045 Polyethylene resin is a premier film resin for heavy duty applications. It complies with U.S. FDA regulation 21 CFR 177.1520 (c) 3.2(a) for food contact applications. The regulation sh.. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | Molded property |
Dow DOWLEX™ 2045.02 Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2045.02 Polyethylene resin is a premier film resin for general packaging applications ranging from heavy duty applications to high speed, thin gauge applications. It contains high level of .. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | Molded property |
Dow DOWLEX™ 2045.02AC Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2045.02AC Polyethylene resin is a high stability blown film extrusion resin that provides excellent tear strength and outstanding toughness. It contains high level of slip additive and medi.. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | Molded property |
Dow DOWLEX™ 2045.11 Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2045.11 Polyethylene resin is a premier film resin for general purpose packaging applications, ranging from heavy duty applications to high speed, thin gauge applications. It contains high .. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | Molded property |
Dow DOWLEX™ 2045A Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2045A Polyethylene blown film extrusion resin is a premier film resin for heavy duty applications. It is utilized where improved thermal stability over a broader range of processing conditi.. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | Molded property |
Dow DOWLEX™ 2056A Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2056A Polyethylene is a premier polymer for heavy duty blown film applications. It is a low gel, high consistency polymer with improved thermal stability and is an outstanding choice for cr.. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | Molded property |
Dow DOWLEX™ 2245A Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2245A Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245A resin is used where improved thermal stability over a broad range of processing conditions is nece.. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | Molded property |
Dow DOWLEX™ 2245D Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2245D Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245D resin is used where improved thermal stability over a broad range of processing conditions is nece.. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | ASTM D638 |
DuPont™ Surlyn® 7930 Ionomer Resin, Lithium Surlyn® 7930 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with lithium ions. The amount of MAA and ne.. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | |
Dymax 3070 Solvent-Free Plastic Adhesive Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide .. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | |
Dymax 3-20556 Solvent-Free Plastic Adhesive Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide .. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | ASTM D638 |
Adell RQ-14 Copolymer Polypropylene, 20% Mica Reinforced Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | |
BCC Products MB 2001 Urethane Foam Modeling Board MB2001 is a general purpose light weight urethane board engineered specifically to meet the tooling requirements of a wide range of applications for the automotive/aerospace, prototype, foundry, and.. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | ASTM D638 |
Buckeye Polymers BP Flex D8020 UC85 TPO TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a.. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | ASTM D412 |
BCC Products BC 8160 Urethane Casting BC8160 is a low viscosity two-component urethane casting compound that is specifically formulated for its flexural and impact strength. It is recommended for use for the production casting of highly.. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | ASTM D412 |
BCC Products BC 8860 Polyurethane Elastomer BC8860 is a low viscosity two-component urethane casting compound that is specifically formulated for high abrasion and impact resistance. It is recommended for use for the production casting of hig.. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | ASTM D412 |
BCC Products BC 8870 Polyurethane Elastomer BC8870 is a low viscosity two-component urethane casting compound that is specifically formulated for high abrasion and impact resistance. It is recommended for use for the production casting of hig.. |
|||
Tensile Strength, Ultimate | 26.2 MPa | 3800 psi | ASTM D638 |
DuPont™ Surlyn® 7940 Ionomer Resin, Lithium Surlyn® 7940 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with lithium ions. The amount of MAA and ne.. |
|||
Tensile Strength, Ultimate | 26.2 - 44.8 MPa | 3800 - 6500 psi | Average value: 41.1 MPa Grade Count:5 |
Overview of materials for Polypropylene with Glass Fiber + PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + PTFE". Each property range of values reported is minimum and maximum va.. |