Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1790 MPa | 260000 psi | |
Latrobe Dynaflex® VAC-ARC High Strength Alloy Steel DYNAFLEX VAC-ARC steel is a medium alloyed, air hardening ultra high strength grade designed for structural applications requiring room temperature tensile strengths of 220,000 to 300,000 psi. Due .. |
|||
Tensile Strength, Ultimate | 1790 MPa | 260000 psi | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 47% Cold Reduction (Coil Spring Range) 45-48% cold reduction is the normal coil spring range. The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.Ge.. |