Polymer Property : Tensile Strength, Ultimate = 261 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 261 MPa
37900 psi
ASTM D638
Quantum Composites QC-8560 60% Glass Fiber Vinyl Ester SMC
QC-8560 is a vinyl ester based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It maintains excellent mechanical properties at temper..
Tensile Strength, Ultimate 261 MPa

@Temperature 760 °C
37900 psi

@Temperature 1400 °F
ATI Allegheny Ludlum 316Ti Austenitic Stainless Steel
Characteristics:excellent resistance to general corrosion, excellent resistance to pitting/crevice corrosion, resistant to sensitization, better creep stress-rupture and tensile strength at elevated..