Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 279 MPa

@Thickness 5.00 mm,
Temperature 100 °C
40500 psi

@Thickness 0.197 in,
Temperature 212 °F
Typical L-T Direction
Aleris HOGAL 5558 Aluminum 5026 H14/H34
HOGAL 5558 is produced according to EN AW-5026.Information provided by Aleris.