Polymer Property : Tensile Strength, Ultimate = 2860 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 19.7 MPa
2860 psi
2 in/min.; ASTM D638
Ineos H28E-00 Polypropylene Homopolymer, Antistatic
Grade H28E-00 is an antistated, controlled rheology polypropylene homopolymer. It is designed for injection molding applications that require improved impact. This material meets the Food and Drug..