Material Notes:
Grade H28E-00 is an antistated, controlled rheology polypropylene homopolymer. It is designed for injection molding applications that require improved impact. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 19.7 MPa
2860 psi
2 in/min.; ASTM D638
Tensile Strength, Yield 34.5 MPa
5000 psi
2 in/min (50 mm/min); ASTM D-638
Elongation at Break 480 %
480 %
2 in/min (50 mm/min); ASTM D-638
Elongation at Yield 10 %
10 %
2 in/min.; ASTM D638
Modulus of Elasticity 0.965 GPa
140 ksi
ASTM D638
Flexural Modulus 1.379 GPa
200.0 ksi
Secant @ 1% strain; ASTM D790
Impact Test 7.10 J
5.24 ft-lb
TUP Impact; 1" radius tip on 1/16" plaque
Descriptive Properties Value Comments
Process Injection Molding