Polymer Property : Tensile Strength, Ultimate = 299.9 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2.068 MPa
299.9 psi
Typical properties based on film cast from toluene solution.; ASTM D412
Kraton® G1702 H (SEP) DiBlock Copolymer
Description: Kraton G1702 H is a clear, linear diblock copolymer based on styrene and ethylene/propylene with a polystyrene content of 28%. It is supplied from North America in the physical form ide..