Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 3.34 MPa
485 psi
Dow Corning SILASTIC® 591 LSR PART A&B
50 Durometer, 2-part, 1 to 1 mix, off-white, Liquid Silicone Rubber, for insulating sleeve and printing roller appliacations.Information provided by Dow Corning
Tensile Strength, Ultimate 3.34 MPa
485 psi
silicone property; ASTM D412
Arlon Thermabond® 99950N008 Silicone Rubber/Fiberglass Laminate
Electrically conductive, Thermabond®. primerless. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.
Tensile Strength, Ultimate 3.34 MPa
485 psi
silicone property; ASTM D412
Arlon Thermabond® 99950N015 Silicone Rubber/Fiberglass Laminate
Electrically conductive, Thermabond®. primerless. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.