Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 3.34 MPa | 485 psi | |
Dow Corning SILASTIC® 591 LSR PART A&B 50 Durometer, 2-part, 1 to 1 mix, off-white, Liquid Silicone Rubber, for insulating sleeve and printing roller appliacations.Information provided by Dow Corning |
|||
Tensile Strength, Ultimate | 3.34 MPa | 485 psi | silicone property; ASTM D412 |
Arlon Thermabond® 99950N008 Silicone Rubber/Fiberglass Laminate Electrically conductive, Thermabond®. primerless. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass. |
|||
Tensile Strength, Ultimate | 3.34 MPa | 485 psi | silicone property; ASTM D412 |
Arlon Thermabond® 99950N015 Silicone Rubber/Fiberglass Laminate Electrically conductive, Thermabond®. primerless. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass. |