Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 2100 MPa | 304000 psi | |
Latrobe Marvac 300 VIM-VAR ; 6.25 in. High Strength Maraging Steel MARVAC 300 VIM-VAR is a low carbon maraging steel capable of 270,000 psi minimum yield strength, coupled with excellent toughness and ductility. The alloy has good fabrication characteristics, which.. |