Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 24.8 MPa | 3600 psi | ASTM D638 |
Chevron Phillips HiD® 9075 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear copolymer; ASTM D3350 Classification 335540A; ASTM D4976 Classification: PE 235, A 54607Characteristics: excellent flow, moderate impact strength, good stiffness, moderate ESCR, e.. |
|||
Tensile Strength, Ultimate | 24.8 MPa | 3600 psi | |
Sylvin Technologies 9604-90C Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 24.8 MPa | 3600 psi | ASTM D638 |
DuPont™ Surlyn® 9910 Ionomer Resin, Zinc Surlyn® 9910 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Tensile Strength, Ultimate | 24.8 MPa | 3600 psi | Molded property |
Dow DOWLEX™ 2049 Linear Low Density Polyethylene, Food Grade DOWLEX® 2049 Polyethylene resin offers excellent tear strength, medium stiffness, outstanding toughness and puncture resistance for films used in food contact applications. When used unmodified and.. |
|||
Tensile Strength, Ultimate | 24.8 MPa | 3600 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8450 Polyolefin Elastomer Description: Engage® 8450 polyolefin elastomer is an ethyleneoctene copolymer that performs well in a wide range of thermoplastic elastomer applications. It has excellent compatibility with other p.. |
|||
Tensile Strength, Ultimate | 24.8 MPa | 3600 psi | ASTM D412 |
Colorite Polymers CS1533UL Wire and Cable Jacket Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 24.8 MPa | 3600 psi | ASTM D412 |
Colorite Polymers CS1534SR Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 24.8 MPa | 3600 psi | ASTM D638 |
Colorite Polymers 92-1107 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 24.8 MPa | 3600 psi | 2 in/min (50 mm/min); ASTM D638 |
Bapolene® 4012 Polypropylene, Extrusion Grade Bapolene PP4012 is a general purpose extrusion resin with excellent stiffness and processability, chemical resistance, and ESCR properties. This product meets FDA standards for food contact applic.. |
|||
Tensile Strength, Ultimate | 24.8 MPa | 3600 psi | ASTM D412/D638 |
Lubrizol ESTANE® 58224 Ester Based Thermoplastic Polyurethane Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 24.8 MPa | 3600 psi | ASTM D638 |
Buckeye Polymers BP RPP 1010 TR Blk Reprocessed Polypropylene, 10% Mineral Filled Talc Filled BlackThis reprocessed product is successful in applications where cost is a major specification, yet physical characteristics require product performance. Industrial recycled resin comp.. |