Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips HiD® 9075 HDPE Injection Molding Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips HiD® 9075 HDPE Injection Molding Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: linear copolymer; ASTM D3350 Classification 335540A; ASTM D4976 Classification: PE 235, A 54607Characteristics: excellent flow, moderate impact strength, good stiffness, moderate ESCR, excellent shrinkage resistanceApplications: thin wall food containers, stadium cupsInformation provided by Chevron Phillips Chemical Company.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D4883
Apparent Bulk Density 0.590 g/cc
0.0213 lb/in³
ASTM D1895
Melt Flow 75 g/10 min

@Load 2.16 kg,
Temperature 190 °C
75 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ASTM D2240
Tensile Strength, Ultimate 24.8 MPa
3600 psi
ASTM D638
Tensile Strength, Yield 24.8 MPa
3600 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Modulus 0.931 GPa
135 ksi
2% Secant; ASTM D 790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ASTM D648
Vicat Softening Point 115 °C
239 °F
ASTM D1525