Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 37.6 MPa | 5450 psi | |
Indium Corp. Indalloy® 10 Pb-In Solder Alloy Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics.. |
|||
Tensile Strength, Ultimate | 37.6 MPa | 5460 psi | |
Williams Advanced Alloys WS240 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Tensile Strength, Ultimate | 37.6 MPa | 5450 psi | |
Williams Advanced Alloys WS264 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Tensile Strength, Ultimate | 37.6 MPa | 5450 psi | after optimum cure |
Armstrong A-12 Epoxy Adhesive, at 3:2 Mix Ratio Our most popular general-purpose, high viscosity adhesive for industry. Combines low toxicity with excellent physical properties, and offers a non-critical mixing ratio of 1:1 by weight. This rati.. |