Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 47.1 MPa | 6830 psi | ASTM D638 |
Kolon DIAMAT® IM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Tensile Strength, Ultimate | 47.1 MPa @Temperature 23.0 °C |
6830 psi @Temperature 73.4 °F |
ASTM D638 |
IRPC Polimaxx Porene GA300 Acrylonitrile Butadiene Styrene Applications: injection molding for electrical appliances, toys. |
|||
Tensile Strength, Ultimate | 47.1 MPa | 6830 psi | ASTM D412 |
SK Chemicals SKYTHANE® X585A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tensile Strength, Ultimate | 47.1 MPa | 6830 psi | ASTM D412 |
SK Chemicals SKYTHANE® 585A X series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Ultimate | 47.1 MPa | 6830 psi | ISO 527 |
Lubrizol Estane® GP 58 DT Thermoplastic Polyurethane Type: Estane® GP 58DT is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding parts, animal identification tagsAvailable in E.. |
|||
Tensile Strength, Ultimate | 47.1 - 53.6 MPa | 6830 - 7770 psi | UV Postcure; ASTM D638M |
DSM Somos® BioClear Parts created with Somos® BioClear are designed for medical applications that are non-implant and have limited contact with the body such as device prototyping. They are shatter-resistant so they w.. |