Tensile Strength, Ultimate 47.1 - 53.6 MPa
6830 - 7770 psi
UV Postcure; ASTM D638M
DSM Somos® BioClear
Parts created with Somos® BioClear are designed for medical applications that are non-implant and have limited contact with the body such as device prototyping. They are shatter-resistant so they w..