Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 47.6 MPa | 6900 psi | ASTM Data |
Americas Styrenics Styron® 678C Polystyrene
(discontinued **) STYRON® 678C general purpose polystyrene resin is a high flow, medium strength resin with good scuff resistance. It is typically used in thin-wall or consumer electronic applications. When used unm.. |
|||
Tensile Strength, Ultimate | 47.6 MPa | 6900 psi | ASTM D638 |
American Polymers API 395 Polystyrene API 395 is one of the highest flowing crystal polystyrenes commercially available. It is produced in pellet form for injection molding and compounding. This material is designed for hard to fill .. |
|||
Tensile Strength, Ultimate | 47.6 MPa | 6900 psi | ASTM D638 |
Eastman Tenite Butyrate 285A2R30016 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 8%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |