Polymer Property : Tensile Strength, Ultimate = 6900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 47.6 MPa
6900 psi
ASTM Data
Americas Styrenics Styron® 678C Polystyrene  (discontinued **)
STYRON® 678C general purpose polystyrene resin is a high flow, medium strength resin with good scuff resistance. It is typically used in thin-wall or consumer electronic applications. When used unm..
Tensile Strength, Ultimate 47.6 MPa
6900 psi
ASTM D638
American Polymers API 395 Polystyrene
API 395 is one of the highest flowing crystal polystyrenes commercially available. It is produced in pellet form for injection molding and compounding. This material is designed for hard to fill ..
Tensile Strength, Ultimate 47.6 MPa
6900 psi
ASTM D638
Eastman Tenite Butyrate 285A2R30016 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 8%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..