Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 250 - 330 MPa
36300 - 47900 psi
SSAB Tunnplat Docol® 4D Deep-drawing Steel
Deep-drawing SteelComments: Docol - Cold Rolled Mild Steel. Property values are for cold-rolled steel; thicknesses 0.40 - 3.00 mm. Iron content is approximate - exact composition is not reported b..
Tensile Strength, Ultimate 270 - 330 MPa
39200 - 47900 psi
SSAB Tunnplat Docol® DC05 (Fe P05) Deep-drawing Steel
Deep-drawing SteelComments: Docol - Cold Rolled Mild Steel. Property values are for cold-rolled steel; thicknesses 0.40 - 3.00 mm. Iron content is approximate - exact composition is not reported b..
Tensile Strength, Ultimate 270 - 330 MPa
39200 - 47900 psi
ArcelorMittal 06 High formability steel for drawing, Cold rolled
Available in the following: uncoated (DC06) and electroglavanized (DC06+ZE) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These product..
Tensile Strength, Ultimate 270 - 330 MPa
39200 - 47900 psi
ArcelorMittal 05 High formability steel for drawing, Cold rolled
Available in the following: uncoated (DC05) and electroglavanized (DC05+ZE) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These product..
Tensile Strength, Ultimate 270 - 330 MPa
39200 - 47900 psi
ArcelorMittal 56 High formability steel for drawing, Cold rolled
Available in the following: Extragal®/Galvannealed (DX56D +Z/+ZF)Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used..
Tensile Strength, Ultimate 270 - 330 MPa
39200 - 47900 psi
ArcelorMittal 57 High formability steel for drawing, Cold rolled
Available in the following: Extragal®/Galvannealed (DX57D +Z/+ZF)Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used..