SSAB Tunnplat Docol® DC05 (Fe P05) Deep-drawing Steel

Category Metal , Ferrous Metal , Carbon Steel , Low Carbon Steel
Manufacturer SSAB Tunnplat AB
Trade Name Docol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SSAB Tunnplat Docol® DC05 (Fe P05) Deep-drawing Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Deep-drawing SteelComments: Docol - Cold Rolled Mild Steel. Property values are for cold-rolled steel; thicknesses 0.40 - 3.00 mm. Iron content is approximate - exact composition is not reported by the manufacturer.Data provided by SSAB Tunnplat.
Physical Properties Metric English Comments
Density 7.87 g/cc
0.284 lb/in³
Estimated by MatWeb
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 270 - 330 MPa
39200 - 47900 psi
Tensile Strength, Yield >= 180 MPa

@Strain 0.200 %
>= 26100 psi

@Strain 0.200 %
Elongation at Break >= 40 %
>= 40 %
A<sub>80</sub>
Component Elements Properties Metric English Comments
Iron, Fe 98 %
98 %