Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 39.2 - 53.0 MPa | 5690 - 7690 psi | Average value: 47.9 MPa Grade Count:13 |
Overview of materials for PCTG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Tensile Strength, Ultimate | 33.0 - 53.0 MPa | 4790 - 7690 psi | Average value: 43.6 MPa Grade Count:28 |