Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 469 - 545 MPa
68000 - 79000 psi
Eagle Brass 510 Phosphor Bronzes 5% A, 3/4 Hard
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
Tensile Strength, Ultimate 476 - 545 MPa
69000 - 79000 psi
Eagle Brass 735 Nickel Silver 18%, 3/4 Hard
735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company
Tensile Strength, Ultimate 360 - 545 MPa
52200 - 79000 psi
Rm
ALIMEX 7075 T651/T652 Aluminum Alloy Rolled
Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHSolution heat treated, stress-relieved by stretching a controlled amount then artificially aged. / Solution..