Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 469 - 545 MPa | 68000 - 79000 psi | |
Eagle Brass 510 Phosphor Bronzes 5% A, 3/4 Hard Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Tensile Strength, Ultimate | 476 - 545 MPa | 69000 - 79000 psi | |
Eagle Brass 735 Nickel Silver 18%, 3/4 Hard 735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company |
|||
Tensile Strength, Ultimate | 360 - 545 MPa | 52200 - 79000 psi | Rm |
ALIMEX 7075 T651/T652 Aluminum Alloy Rolled Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHSolution heat treated, stress-relieved by stretching a controlled amount then artificially aged. / Solution.. |