Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 39.61 MPa | 5745 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Therma-Tech™ NJC-7500 Nylon 12
(discontinued **) PolyOne First ChoiceInformation provided by PolyOne Corporation. |