Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 0.400 - 220 MPa | 58.0 - 31900 psi | Average value: 6.93 MPa Grade Count:187 |
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum va.. |
|||
Tensile Strength, Ultimate | 0.400 - 6.86 MPa | 58.0 - 995 psi | Average value: 3.53 MPa Grade Count:29 |
Overview of materials for Silicone, RTV, Encapsulation Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Encapsulation Grade". Each property range of values reported is minimum and maximum value.. |
|||
Tensile Strength, Ultimate | 0.400 MPa | 58.0 psi | |
Dow Corning JCR 6115 Two-part, fast cure, low modulus LED encapsulant with low viscosity and very long working time.Information provided by Dow Corning |