Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 5800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 29.0 - 40.0 MPa
4210 - 5800 psi
Average value: 34.4 MPa Grade Count:16
Overview of materials for High Density Polyethylene (HDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max..
Tensile Strength, Ultimate 25.0 - 40.0 MPa
3630 - 5800 psi
Alliance BIN-40 Bonded (Composite) Magnetic Material
Tensile Strength, Ultimate 32.0 - 40.0 MPa
4640 - 5800 psi
ASTM D638
Arkema Group VOLTALEF® 300 HD PCTFE
VOLTALEF® 300 HD is a chlorotrifluoroethylene powder. Used for compression molding, very good flow, non-flammable. Information provided by Arkema Group
Tensile Strength, Ultimate 32.0 - 40.0 MPa
4640 - 5800 psi
ASTM D638
Arkema Group VOLTALEF® 302 PCTFE
VOLTALEF® 302 is a chlorotrifluoroethylene dense powder. Used in particular for compression molding, non-flammable. Information provided by Arkema Group
Tensile Strength, Ultimate 25.0 - 40.0 MPa
3630 - 5800 psi
Alliance BIN-26 Bonded (Composite) Magnetic Material
Tensile Strength, Ultimate 25.0 - 40.0 MPa
3630 - 5800 psi
Alliance BIN-45 Bonded (Composite) Magnetic Material
Tensile Strength, Ultimate 25.0 - 40.0 MPa
3630 - 5800 psi
Alliance BIN-48 Bonded (Composite) Magnetic Material
Tensile Strength, Ultimate 25.0 - 40.0 MPa
3630 - 5800 psi
Alliance BIN-55 Bonded (Composite) Magnetic Material
Tensile Strength, Ultimate 25.0 - 40.0 MPa
3630 - 5800 psi
Alliance BIN-72 Bonded (Composite) Magnetic Material
Tensile Strength, Ultimate 20.0 - 40.0 MPa
2900 - 5800 psi
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 11008 PVDF Copolymer  (discontinued **)
Key features of this grade: Low Viscosity, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVD..
Tensile Strength, Ultimate 18.0 - 40.0 MPa

@Temperature 60.0 - 120 °C
2610 - 5800 psi

@Temperature 140 - 248 °F
Average value: 29.3 MPa Grade Count:1
Overview of materials for Polypropylene with Glass Fiber + Bead Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max..
Copyright © lookpolymers.com All Rights Reserved