Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 480 - 590 MPa
69600 - 85600 psi
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; H (TD04) Temper; up to 76 mm Thickness (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 410 - 590 MPa
59500 - 85600 psi
Materion Beryllium Copper Alloy 165 Forgings & Extrusions; A (TB00) Temper (UNS C17000)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 410 - 590 MPa
59500 - 85600 psi
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; A (TB00) Temper; All Thicknesses (UNS C17000)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 410 - 590 MPa
59500 - 85600 psi
Materion Beryllium Copper Alloy 165 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17000)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 410 - 590 MPa
59500 - 85600 psi
Materion Beryllium Copper Alloy 25 Forgings & Extrusions; A (TB00) Temper (UNS C17200)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 410 - 590 MPa
59500 - 85600 psi
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; A (TB00) Temper; All Thicknesses (UNS C17200)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 410 - 590 MPa
59500 - 85600 psi
Materion Beryllium Copper Alloy 25 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17200)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 410 - 590 MPa
59500 - 85600 psi
Materion Beryllium Copper Alloy 25 Tube; A (TB00) Temper; All Sizes (UNS C17200)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 410 - 590 MPa
59500 - 85600 psi
Materion Beryllium Copper Alloy M25 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17300)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 470 - 590 MPa
68200 - 85600 psi
ArcelorMittal HSLA 420 High strength low alloy steel for cold forming, Cold Rolled
Available in the following: uncoated (HC420LA), electroglavanized (HC420LA +ZE) and Extragal®/galfan/Galvannealed (HC420LA+Z/+ZA/+ZF)Description: Steels in the HSLA (High Strength Low Alloy) range ..
Tensile Strength, Ultimate 460 - 590 MPa
66700 - 85600 psi
Rm
ALIMEX AMP 8000 Aluminum Plate
AMP 8000 offers higher strength levels, good machinability and dimensional stability. Its tensile strength is up to 40% higher than AlZn5.5MgCu (7075). Moulding, (Prototypes) injection moulds, Jig ..
Tensile Strength, Ultimate 480 - 590 MPa
69600 - 85600 psi
Materion Beryllium Copper Alloy 3 Plate & Rolled Bar; H (TD04) Temper; up to 76 mm Thickness (UNS C17510)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..