Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 595 MPa | 86300 psi | Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4550 Austenitic Stainless Steel Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto) and rod forms. |
|||
Tensile Strength, Ultimate | 595 MPa | 86300 psi | Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4841 High Temperature Austenitic Stainless Steel Variant of 1.4845 with an increased silicon content which enhances the steel's resistance to oxidation/corrosion but has also made it more susceptible to embrittlement.Applications: Heat and creep r.. |
|||
Tensile Strength, Ultimate | 595 MPa | 86300 psi | Calculated from tenacity |
DuPont™ Nomex® 430 1600 Denier Aramid Yarn A high crystallinity natural filament yarn of NOMEX with higher strength and chemical resistance than staple spun yarns. Type 430 is used where the aesthetics and properties of a filament yarn are .. |
|||
Tensile Strength, Ultimate | 595 MPa | 86300 psi | Typical |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Annealed Allegheny Ludlum Type 425 Mod is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stai.. |