Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 415 MPa
>= 60200 psi
MetalTek C18100 Chrome Zirc Copper High Conductivity
Typical property data from forged samples.Information provided by MetalTekCast UNS C18100; Cast Grade C18100
Tensile Strength, Ultimate >= 415 MPa
>= 60200 psi
MetalTek MTEK 10-60 Cast UNS N08001 Heat Resistant Stainless Steel
Not as strong as HT but high nickel content delivers excellent carburization resistance.Applications: Cyanide pots, retorts, molten lead heating elements.Information provided by MetalTekCast UNS N08..
Tensile Strength, Ultimate >= 415 MPa
>= 60200 psi
MetalTek MTEK 15-65 Cast UNS N06006 Heat Resistant Stainless Steel
For severe hot gas corrosion resistance at higher temperatures.Applications: Hearth plates, muffles, roller hearths, carburizing boxes.Information provided by MetalTekCast UNS N06006; Cast Grade HX;..
Tensile Strength, Ultimate 415 MPa

@Temperature 22.0 °C
60200 psi

@Temperature 71.6 °F
25mm flat samples, compression moulded; ISO 527-4
Menzolit Menzolit® HPC 1300 Unsaturated Polyester UP
HPC 1300 is a special SMC for high strength applications. The glass level has been selected to combine mouldability with high strength and stiffness properties in orientation direction. The reinforc..
Tensile Strength, Ultimate >= 415 MPa
>= 60200 psi
MetalTek MTEK 70-30 UNS C96400 Nickel-Copper Alloy
Information provided by MetalTek
Tensile Strength, Ultimate 415 MPa

@Temperature 870 °C
60200 psi

@Temperature 1600 °F
Haynes 188 alloy, cold rolled and 1175°C solution annealed sheet
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Tensile Strength, Ultimate 415 MPa

@Temperature 870 °C
60200 psi

@Temperature 1600 °F
Haynes 25 alloy, cold rolled and 1205°C (2200°F) solution annealed sheet
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Ultimate 415 MPa
60200 psi
Annealed
Special Metals FERRY® Alloy
A copper-nickel alloy used mainly for its electrical properties. It has medium-range electrical resistivity and a very low temperature coefficient of resistance (TCR). The low TCR makes the alloy ..
Tensile Strength, Ultimate >= 415 MPa
>= 60200 psi
AK Steel CL 1/ SAE J1392 045 XLK, Grade 45 Cold Rolled Carbon Steel, High Strength Low Alloy Steel (HSLAS)
Information provided by AK Steel
Tensile Strength, Ultimate >= 415 MPa
>= 60200 psi
AK Steel SAE J1392 050 XLK, Grade 50 Aluminized Carbon Steel, High Strength Low Alloy Steel (HSLAS)
Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate.Information provided by AK Steel
Tensile Strength, Ultimate >= 415 MPa
>= 60200 psi
AK Steel ZINCGRIP® FORMABLE 50K / ASTM A1008 class 2 / SAE J1392 050 XLK, Grade 50 Electrogalvanized Carbon Steel, High Strength Low Alloy Steel (HSLAS)
Information provided by AK Steel
Tensile Strength, Ultimate >= 415 MPa
>= 60200 psi
Minimum
ATI Allegheny Ludlum Stainless Steel AL 410S™ (UNS S41008)
Allegheny Ludlum Al 410S™ stainless steel is a low-carbon modification of Type 410 stainless steel. Low carbon and optionally a small addition of titanium and /or columbium minimize austenite form..
Tensile Strength, Ultimate >= 415 MPa
>= 60200 psi
Minimum
Aleris Weldural Aluminum Alloy, 100 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..
Tensile Strength, Ultimate 415 - 470 MPa
60200 - 68200 psi
ArcelorMittal HSLA 320 High strength low alloy steel for cold forming, Hot Rolled
Available in the following: S315MCDescription: Steels in the HSLA (High Strength Low Alloy) range are hardened by a combination of precipitation and grain size refining, resulting in high strength w..
Copyright © lookpolymers.com All Rights Reserved