Material Notes:
A copper-nickel alloy used mainly for its electrical properties. It has medium-range electrical resistivity and a very low temperature coefficient of resistance (TCR). The low TCR makes the alloy useful for wire-wound precision resistors having operating temperatures up to 750°F (400°C). A reproducible electromotive force against copper makes the alloy suitable for thermocouples and thermocouple compensating leads. Standard product forms are round, sheet, strip, and wire.Data provided by the manufacturer, Special Metals.
Physical Properties Metric English Comments
Density 8.89 g/cc
0.321 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 415 MPa
60200 psi
Annealed
Tensile Strength, Yield 145 MPa

@Strain 0.200 %
21000 psi

@Strain 0.200 %
Annealed
Elongation at Break 32 %
32 %
Annealed
Thermal Properties Metric English Comments
CTE, linear 14.7 µm/m-°C

@Temperature 20.0 - 100 °C
8.17 µin/in-°F

@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.394 J/g-°C
0.0942 BTU/lb-°F
Thermal Conductivity 22.4 W/m-K
155 BTU-in/hr-ft²-°F
Melting Point 1220 - 1270 °C
2230 - 2320 °F
Solidus 1220 °C
2230 °F
Liquidus 1270 °C
2320 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.10 %
<= 0.10 %
Copper, Cu 55 %
55 %
Iron, Fe <= 1.0 %
<= 1.0 %
Manganese, Mn <= 1.0 %
<= 1.0 %
Nickel, Ni 42 %
42 %
As remainder
Silicon, Si <= 0.50 %
<= 0.50 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000490 ohm-cm
0.0000490 ohm-cm
Temperature coefficient of resistance is 30 µOhm/Ohm-°C in the range 25-100°C.