Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 614 MPa

@Temperature 649 °C
89100 psi

@Temperature 1200 °F
Kennametal Stellite Stellite® 31 PM with P/M Processing; heat treated at 93°C (200°F) and water quenched
Typical applications include, miscellaneous wear parts. Data provided by the manufacturer, Deloro Stellite Inc.Product of former Deloro Stellite Inc.
Tensile Strength, Ultimate 614 MPa

@Diameter 12.7 mm
89100 psi

@Diameter 0.500 in
Kaiser 7068 T76, T76511 Rod & Bar
Alloy 7068 offers some of the highest strength mechanical properties available in an extruded product. Intended for aerospace, ordnance and light weight recreational applications where extremely hig..
Tensile Strength, Ultimate 614 MPa

@Temperature 427 °C
89100 psi

@Temperature 801 °F
Haynes Hastelloy® C-22® alloy, 12.7-50.8 mm thick bar, solution heat treated
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Tensile Strength, Ultimate 614 - 669 MPa
89000 - 97000 psi
Eagle Brass 240 Low Brass, Extra Spring
CDA 240 has excellent ductility, corrosion resistance and strength which allows it to be deep drawn, etched, stamped, blanked and bent. Typical uses include musical instruments, battery caps, flexib..
Copyright © lookpolymers.com All Rights Reserved