Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 614 - 669 MPa
89000 - 97000 psi
Eagle Brass 240 Low Brass, Extra Spring
CDA 240 has excellent ductility, corrosion resistance and strength which allows it to be deep drawn, etched, stamped, blanked and bent. Typical uses include musical instruments, battery caps, flexib..