Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 448 MPa
65000 psi
Pacific Sintered Materials FCC-216-P(HT) High Carbon Copper Steel Powdered Metal
High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI..
Tensile Strength, Ultimate 448 MPa
65000 psi
Pacific Sintered Materials FS-1603 Silicon Iron Soft Magnetic Powdered Metal
Applications: DC magnetic applications such as armatures, relays, solenoids, pole pieces and cores. Possible AC uses.All information provided by Pacific Sintered Metals.
Tensile Strength, Ultimate 448 MPa
65000 psi
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-216-P(HT) Powdered Metal
High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP..
Tensile Strength, Ultimate 448 MPa
65000 psi
PSM Industries Pacific Sintered Metals Silicon Iron FS-1603 Powdered Metal
DC magnetic applications such as armatures, relays, solenoids, pole pieces and cores. Possible AC usesInformation Provided by Pacific Sintered Metals, a division of PSM Industries
Tensile Strength, Ultimate 448 MPa
65000 psi
Hogen Duralloy H1W 55 Tungsten/45 Copper PM Metal Composite
RWMA Class 10.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is ..
Tensile Strength, Ultimate 448 MPa
65000 psi
FloMet 304L Stainless Steel
FloMet provides precision miniature components through metal injection molding (MIM). Metal powders are mixed with thermoplastic binders to form a homogeneous mixture, with approximately 60% volume..
Tensile Strength, Ultimate 448 MPa
65000 psi
Mi-Tech Metals CW55 55 Tungsten/45 Copper PM Metal Composite
RWMA Class 10.Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is recomme..
Tensile Strength, Ultimate 448 MPa
65000 psi
1020 Steel butt joint
Lucas-Milhaupt EASY FLO Silver Based Cadmium-Bearing Filler Metal
Applications: Easy-Flo is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wettin..
Tensile Strength, Ultimate 448 - 552 MPa
65000 - 80000 psi
Eagle Brass 725 Copper Nickel Tin, 1/2 Hard
Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina..
Tensile Strength, Ultimate 448 - 558 MPa
65000 - 81000 psi
Eagle Brass 762 Nickel Silver 12%, 1/4 Hard
762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s..
Tensile Strength, Ultimate 448 MPa

@Thickness <=25.0 mm
65000 psi

@Thickness <=0.984 in
Plate
CMW® 3 Copper Alloy
CMW® 3 material is a high strength, high conductivity copper base alloy. CMW® 3 material is heat treatable. Optimum mechanical and physical properties of CMW® 3 material are developed by heat tre..
Tensile Strength, Ultimate 448 MPa
65000 psi
Dura-Bar 65-45-12 HRDS Continuously Cast Ductile Iron Bar Stock ASTM A536
Dura-Bar 4512 HRDS is a high-silicon ductile iron intended for use at elevated temperatures or when a part is subjected to thermal cycling, such as permanent mold applications. The ferritic structu..
Tensile Strength, Ultimate 448 MPa
65000 psi
annealed
CMW® ELKONIUM 306 platinum based alloy
Platinum has complete freedom from atmospheric corrosion and is preferred for devices that have low closed forces and where surety of making a circuit may be a problem. It has a high melting point (..
Tensile Strength, Ultimate 448 MPa
65000 psi
cold worked
CMW® ELKONIUM 73 Copper Cadmium Alloy with Au/Ag-Cladding
ELKONIUM 73 alloy is a silver, copper, cadmium and gold material marketed by CMW with high electrical and thermal properties. It is designed as an economical rivet type contact for AC applications r..
Tensile Strength, Ultimate 448 MPa
65000 psi
AIM 91Sn/9Zn Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.
Tensile Strength, Ultimate 448 MPa

@Temperature 593 °C
65000 psi

@Temperature 1100 °F
Carpenter 20-Mo6® Stainless Steel, Tensile Properties at 93°C
Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, ..
Tensile Strength, Ultimate 448 MPa
65000 psi
Annealed
AK Steel 410S Ferritic Stainless steel
AK Steel 410S Stainless Steel is a non-hardening modification of Type 410. A small titanium addition minimizes austenite formation at high temperatures, thereby restricting the alloy's ability to h..
Tensile Strength, Ultimate 448 MPa
65000 psi
Carpenter Invar 36® Alloy, Annealed Bars and Strip
Data provided by Carpenter Technology Corporation.Carpenter Invar "36" alloy is a 36% nickel-iron alloy possessing a rate of thermal expansion approx. one-tenth that of carbon steel up to 200°C. T..
Tensile Strength, Ultimate 448 MPa
65000 psi
ATI Allvac® 55, Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal
Data provided by Allvac.Applications: Airframe skin, heat exchangers, cryogenic vessels, components for CPI equipment, condenser tubing, exhaust pipe shrouds.
Tensile Strength, Ultimate >= 448 MPa
>= 65000 psi
PSM Industries PolyAlloys MIM-316L sintered Stainless Steel
PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl..
Tensile Strength, Ultimate 448 MPa
65000 psi
ACMA Test #4
CeramTec 965 Toughened Alumina (Al2O3-ZrO2)
Hasselman Thermal Shock value is 270 K.Data provided by CeramTec North America.