Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hogen Duralloy H1W 55 Tungsten/45 Copper PM Metal Composite

Category Metal , Metal Matrix Composite , Nonferrous Metal , Refractory Metal , Tungsten Alloy
Manufacturer Hogen Industries
Trade Name Duralloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hogen Duralloy H1W 55 Tungsten/45 Copper PM Metal Composite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
RWMA Class 10.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is recommended as facings or inserts for projection welding electrodes and for flash and butt welding dies where high electrical conductivity is desirable and relatively high malleability is necessary. H1W and H3W are most commonly used for flash and butt welding die inserts.Data provided by Hogen Industries.
Physical Properties Metric English Comments
Density >= 12.25 g/cc
>= 0.4426 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 73
73
Tensile Strength, Ultimate 448 MPa
65000 psi
Thermal Properties Metric English Comments
CTE, linear 11.8 µm/m-°C

@Temperature 20.0 °C
6.56 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.251 J/g-°C

@Temperature 20.0 °C
0.0600 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 240 W/m-K

@Temperature 20.0 - 400 °C
1670 BTU-in/hr-ft²-°F

@Temperature 68.0 - 752 °F
Component Elements Properties Metric English Comments
Copper, Cu 45 %
45 %
Tungsten, W 55 %
55 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000300 ohm-cm
0.00000300 ohm-cm