Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 70000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 483 MPa
70000 psi
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Hydrogen Annealed at 2150°F (1177°C)
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Tensile Strength, Ultimate 483 MPa
70000 psi
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Hydrogen Annealed at 2150°F (1177°C)
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Tensile Strength, Ultimate 483 MPa
70000 psi
Kinetics MIM 2.5% SiFe Soft Magnetic Steel
Low alloy steel, silicon. A work hardenable steel alloy that offers very good magnetic properties, tensile strength, hardness, wear resistance, and increased spring steel strength. Can be plated or ..
Tensile Strength, Ultimate 483 MPa
70000 psi
FloMet Fe-3% Si Soft Magnetic Alloy
FloMet provides precision miniature components through metal injection molding (MIM). Metal powders are mixed with thermoplastic binders to form a homogeneous mixture, with approximately 60% volume..
Tensile Strength, Ultimate 483 - 517 MPa
70000 - 75000 psi
Materion BrushCAST® 165C High Strength Casting Alloy (As Cast)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Tensile Strength, Ultimate 483 - 517 MPa
70000 - 75000 psi
Materion BrushCAST® 165CT Fine Grain Casting Alloy (As Cast)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Tensile Strength, Ultimate 483 MPa

@Temperature 23.0 °C
70000 psi

@Temperature 73.4 °F
Lucas-Milhaupt EASY FLO Silver Based Cadmium-Bearing Filler Metal
Applications: Easy-Flo is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wettin..
Tensile Strength, Ultimate 483 MPa
70000 psi
Universal Wire Works 190 Nickel Alloy Welding Wire
Alloy 190 is used for arc welding Monel type alloys 400 and 404 to themselves or to one another, as well as overlaying on steel. Typical applications include welding ASTM B127, B163, B164, and B165...
Tensile Strength, Ultimate 483 MPa
70000 psi
Universal Wire Works 60 Nickel Alloy Welding Wire
Alloy 60 is used for Gas Metal Arc Welding (GMAW), Gas Tungsten Arc Welding (GTAW), and Submerged Arc Welding (SMA) of Monel type alloys 400 and 404, as well as overlaying on steel. When GMAW or MIG..
Tensile Strength, Ultimate 483 MPa
70000 psi
Universal Wire Works No. 1 Cobalt Alloy Welding Wire
Universal No. 1 is a cobalt-chromium-tungsten alloy suited for applications requiring extreme abrasion resistance at elevated temperatures. Excellent for resistance to corrosion and oxidation where ..
Tensile Strength, Ultimate 483 - 524 MPa
70000 - 76000 psi
Eagle Brass 194 HSM® Copper, Spring
High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl..
Tensile Strength, Ultimate 483 - 565 MPa
70000 - 82000 psi
Eagle Brass 425 Tin Brass 2%, Hard
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
Tensile Strength, Ultimate 483 - 641 MPa
70000 - 93000 psi
Eagle Brass 64725 MAX251C, 1/2 Hard
Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In..
Tensile Strength, Ultimate 483 MPa
70000 psi
18-20in thickness
Clinton Aluminum Alumold 1-500 Forged
Alumold 1-500 Forged is a high quality, high strength aluminum alloy intended for the plastic forming industry and for other tooling applications. With its high strength and surface hardness it is ..
Tensile Strength, Ultimate 483 MPa
70000 psi
annealed
CMW® ELKONIUM 34 platinum based alloy
Platinum has complete freedom from atmospheric corrosion and is preferred for devices that have low closed forces and where surety of making a circuit may be a problem. It has a high melting point (..
Tensile Strength, Ultimate 483 MPa
70000 psi
annealed
CMW® ELKONIUM 405 palladium based alloy
Palladium belongs to the platinum group of metals and like platinum is highly resistant to atmospheric corrosion; however, it begins to tarnish at temperatures above 400(C. It has a high melting poi..
Tensile Strength, Ultimate 483 MPa
70000 psi
Semi-Processed
AK Steel DI-MAX® M-43 Nonoriented Electrical Steel
Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard grades from M-15 to M-47 ..
Tensile Strength, Ultimate 483 MPa
70000 psi
Carpenter Super Invar 32-5
Carpenter Super Invar 32-5, a magnetic, austenitic, solid solution alloy containing iron, nickel and cobalt, is designed to provide minimum thermal expansion at room temperatures. This alloy also e..
Tensile Strength, Ultimate 483 MPa
70000 psi
90° stress angle
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Crossply
CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li..
Tensile Strength, Ultimate 483 MPa
70000 psi
0° stress angle
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Crossply
CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li..
Copyright © lookpolymers.com All Rights Reserved