Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 441 - 490 MPa | 64000 - 71000 psi | |
Eagle Brass 151 ZHC® COPPER, Spring Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c.. |
|||
Tensile Strength, Ultimate | 421 - 490 MPa | 61000 - 71000 psi | |