Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 421 MPa | 61000 psi | |
Pacific Sintered Materials SS-316-RD 316L Stainless Steel Powdered Metal Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance.Equivalent MPIF Specification: SS-316-40All information provided by Pacific Sin.. |
|||
Tensile Strength, Ultimate | 421 MPa | 61000 psi | |
PSM Industries Pacific Sintered Metals 316L Stainless Steel SS-316-RD Powdered Metal Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance. Equivalent MPIF Specification: SS-316-40Information Provided by Pacific Sinte.. |
|||
Tensile Strength, Ultimate | 421 MPa @Temperature 760 °C |
61100 psi @Temperature 1400 °F |
|
Haynes HR-160® alloy, solution annealed sheet Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Tensile Strength, Ultimate | 421 - 510 MPa | 61000 - 74000 psi | |
Eagle Brass 18665 MSP1, 1/2 Hard MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs.. |
|||
Tensile Strength, Ultimate | 421 - 476 MPa | 61000 - 69000 psi | |
Eagle Brass 210 Gilding Metal, Extra Spring CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Tensile Strength, Ultimate | 421 - 490 MPa | 61000 - 71000 psi | |
Eagle Brass 240 Low Brass, 3/4 Hard CDA 240 has excellent ductility, corrosion resistance and strength which allows it to be deep drawn, etched, stamped, blanked and bent. Typical uses include musical instruments, battery caps, flexib.. |
|||
Tensile Strength, Ultimate | 421 - 524 MPa | 61000 - 76000 psi | |
Eagle Brass 519 Phosphor Bronzes 6%, 1/2 Hard Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Tensile Strength, Ultimate | 421 - 524 MPa | 61000 - 76000 psi | |
Eagle Brass 770 Nickel Silver 18%, Annealed 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Tensile Strength, Ultimate | 421 MPa | 61100 psi | |
Carpenter Chrome Core® 12 Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |
|||
Tensile Strength, Ultimate | 421 MPa | 61100 psi | |
Carpenter Chrome Core® 8 Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |
|||
Tensile Strength, Ultimate | 421 MPa | 61100 psi | |
Ametek High Purity Nickel Strip 899E Annealed Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Ultimate | 421 MPa | 61100 psi | |
Carpenter Chrome Core® 8-FM Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |
|||
Tensile Strength, Ultimate | 421 MPa | 61100 psi | |
Carpenter Chrome Core® 12-FM Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |