Polymer Property : Tensile Strength, Ultimate = 7300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 14.3 - 50.3 MPa
2080 - 7300 psi
Average value: 38.0 MPa Grade Count:56
Overview of materials for PVC, Rigid Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M..
Tensile Strength, Ultimate 36.3 - 50.3 MPa
5270 - 7300 psi
Average value: 43.2 MPa Grade Count:11
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim..