Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.08 - 1.17 g/cc
0.0390 - 0.0423 lb/in³
Average value: 1.13 g/cc Grade Count:13
Water Absorption 0.300 - 2.00 %
0.300 - 2.00 %
Average value: 0.709 % Grade Count:9
Linear Mold Shrinkage 0.00300 - 0.00800 cm/cm
0.00300 - 0.00800 in/in
Average value: 0.00543 cm/cm Grade Count:7
Melt Flow 1.60 - 12.0 g/10 min
1.60 - 12.0 g/10 min
Average value: 5.35 g/10 min Grade Count:13
Mechanical Properties Metric English Comments
Hardness, Rockwell M 27.0 - 60.0
27.0 - 60.0
Average value: 37.8 Grade Count:6
Tensile Strength, Ultimate 36.3 - 50.3 MPa
5270 - 7300 psi
Average value: 43.2 MPa Grade Count:11
Elongation at Break 5.00 - 50.0 %
5.00 - 50.0 %
Average value: 24.0 % Grade Count:13
Elongation at Yield 3.60 - 4.50 %
3.60 - 4.50 %
Average value: 3.99 % Grade Count:7
Modulus of Elasticity 1.38 - 2.96 GPa
200 - 430 ksi
Average value: 2.06 GPa Grade Count:13
Flexural Yield Strength 46.9 - 85.5 MPa
6800 - 12400 psi
Average value: 64.8 MPa Grade Count:11
Flexural Modulus 1.65 - 2.45 GPa
240 - 355 ksi
Average value: 2.08 GPa Grade Count:7
Izod Impact, Notched 0.320 - 1.23 J/cm
0.600 - 2.30 ft-lb/in
Average value: 0.776 J/cm Grade Count:11
0.42712 - 0.58729 J/cm

@Temperature 0.000 - 0.000 °C
0.80017 - 1.1002 ft-lb/in

@Temperature 32.0 - 32.0 °F
Average value: 0.534 J/cm Grade Count:3
0.42712 - 0.58729 J/cm

@Diameter 6.35 - 6.35 mm
0.80017 - 1.1002 ft-lb/in

@Diameter 0.250 - 0.250 in
Average value: 0.534 J/cm Grade Count:3
Gardner Impact 3.05 - 7.34 J
2.25 - 5.42 ft-lb
Average value: 5.20 J Grade Count:4
Thermal Properties Metric English Comments
CTE, linear 72.0 - 100 µm/m-°C
40.0 - 55.6 µin/in-°F
Average value: 88.4 µm/m-°C Grade Count:7
Deflection Temperature at 0.46 MPa (66 psi) 85.0 - 90.0 °C
185 - 194 °F
Average value: 87.6 °C Grade Count:4
Deflection Temperature at 1.8 MPa (264 psi) 70.0 - 85.6 °C
158 - 186 °F
Average value: 78.9 °C Grade Count:13
Vicat Softening Point 80.0 - 112 °C
176 - 234 °F
Average value: 95.1 °C Grade Count:13
Flammability, UL94 HB
HB
Grade Count:7
Optical Properties Metric English Comments
Refractive Index 1.49 - 1.51
1.49 - 1.51
Average value: 1.50 Grade Count:5
Haze 2.00 - 7.00 %
2.00 - 7.00 %
Average value: 4.29 % Grade Count:7
Yellow Index -1.00 - -0.300 %
-1.00 - -0.300 %
Average value: -0.440 % Grade Count:5
Transmission, Visible 80.0 - 91.0 %
80.0 - 91.0 %
Average value: 88.0 % Grade Count:13
Processing Properties Metric English Comments
Melt Temperature 182 - 249 °C
360 - 480 °F
Average value: 223 °C Grade Count:5
Mold Temperature 48.9 - 82.2 °C
120 - 180 °F
Average value: 65.6 °C Grade Count:5
Drying Temperature 71.1 - 79.4 °C
160 - 175 °F
Average value: 74.4 °C Grade Count:5