Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 655 - 758 MPa | 95000 - 110000 psi | |
Eagle Brass 510 Phosphor Bronzes 5% A, Spring Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Tensile Strength, Ultimate | 621 - 758 MPa | 90000 - 110000 psi | |
Eagle Brass 7026 Copper Nickel, 1/2 Hard 7026 is a high performance alloy used in springs, terminals, elevated temperature interconnects and high reliability telecommunication components.Information provided by Eagle Brass Company |
|||
Tensile Strength, Ultimate | 621 - 758 MPa | 90000 - 110000 psi | |
Eagle Brass 70265 XP175, 1/2 Hard Information provided by Eagle Brass Company |