Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 53.1 MPa
7700 psi
ASTM D412
Lubrizol Estane® ALR E87A Thermoplastic Polyurethane
Type: Estane® ALR E87A is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corpor..
Tensile Strength, Ultimate 53.1 MPa
7700 psi
ASTM D412/D638
Lubrizol ESTANE® 58138 Ester Based Thermoplastic Polyurethane
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tensile Strength, Ultimate 53.1 MPa
7700 psi
after optimum cure
Armstrong C-1/H20 Epoxy Adhesive
A versatile, low viscosity, unfilled resin used for electrical potting and laminating applications. It is an excellent insulator, and provides outstanding chemical resistance to most compoundsInfor..