Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 531 MPa | 77000 psi | |
Pacific Sintered Materials FX-227-T Infiltrated Steel Powdered Metal Machines and plates well. Good in hydraulic applications. Moderate tolerance control.Equivalent MPIF Specification: FX-1005-50All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Ultimate | 531 MPa | 77000 psi | |
PSM Industries Pacific Sintered Metals Infiltrated Steel FX-227-T Powdered Metal Machines and plates well, Good in hydraulic applications, Moderate tolerance control Equivalent MPIF Specifications: FX-1005-50Information Provided by Pacific Sintered Metals, a division of PSM Ind.. |
|||
Tensile Strength, Ultimate | 531 MPa | 77000 psi | |
PSM Industries PolyAlloys MIM-Fe-%3Si Grade 2 Soft Magnetic Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Tensile Strength, Ultimate | 531 MPa | 77000 psi | Heat Treated |
Universal Wire Works 410 Stainless Steel (AMS 5776) Filler Metal Universal 410 is a ferritic stainless steel alloy, primarily used as filler metal for gas metal arc and gas tungsten arc welding of steel of similar composition. Deposits are resistant to corrosion .. |
|||
Tensile Strength, Ultimate | 531 MPa @Temperature 21.1 °C |
77000 psi @Temperature 70.0 °F |
annealed bar |
Crucible Steel 430F Stainless Steel Crucible 430F is a low carbon, high chromium ferritic stainless steel, specially developed for solenoid core applications in corrosive environments. The chemistry is closely controlled to develop o.. |
|||
Tensile Strength, Ultimate | 531 MPa @Temperature 538 °C |
77000 psi @Temperature 1000 °F |
|
Carpenter 20Cb-3® Stainless Steel Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Tensile Strength, Ultimate | 531 MPa @Temperature 260 °C |
77000 psi @Temperature 500 °F |
|
Carpenter 20-Mo6® Stainless Steel, Tensile Properties at 93°C Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, .. |
|||
Tensile Strength, Ultimate | 531 MPa @Temperature 427 °C |
77000 psi @Temperature 801 °F |
ASTM E8 |
ATI Allegheny Ludlum 309S Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Tensile Strength, Ultimate | 530.9 MPa | 77000 psi | |
ATI Allegheny Ludlum Relay Steels No. 5 Silicon and iron alloyApplications:relays, armatures, solenoids, magnetic clutches, pole pieces, certain types of motors, transformers, data processing equipment.Information provided by Allegheny Lu.. |
|||
Tensile Strength, Ultimate | 531 MPa @Temperature 482 °C |
77000 psi @Temperature 900 °F |
|
Carpenter Gall-Tough® Stainless Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 1.. |
|||
Tensile Strength, Ultimate | 531 MPa | 77000 psi | |
Carpenter HyMu "80"® Electronic Alloy, Hydrogen Annealed Strip Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
Tensile Strength, Ultimate | 531 MPa | 77000 psi | Typical; Annealed at 2100°F (1149°C) |
ATI Allegheny Ludlum AL 800AT™ Nickel-Base Alloy, UNS N08811 AL 800AT alloy is nickel-iron-chromium alloys designed to resist oxidation and carburization at elevated temperatures. The nickel content makes the alloy highly resistant both to chloride stress-co.. |
|||
Tensile Strength, Ultimate | 531 MPa | 77000 psi | Typical; Annealed at 2100°F (1149°C) |
ATI Allegheny Ludlum AL 800H™ Nickel-Base Alloy, UNS N08810 AL 800H alloy is nickel-iron-chromium alloys designed to resist oxidation and carburization at elevated temperatures. The nickel content makes the alloy highly resistant both to chloride stress-cor.. |
|||
Tensile Strength, Ultimate | 531 MPa | 77000 psi | |
PSM Industries PolyAlloys MIM-Fe-%3Si Grade 1 Soft Magnetic Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |