Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Universal Wire Works 410 Stainless Steel (AMS 5776) Filler Metal

Category Metal , Ferrous Metal , Stainless Steel
Manufacturer Universal Wire Works
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works 410 Stainless Steel (AMS 5776) Filler Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Universal 410 is a ferritic stainless steel alloy, primarily used as filler metal for gas metal arc and gas tungsten arc welding of steel of similar composition. Deposits are resistant to corrosion and moderate heat.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 531 MPa
77000 psi
Heat Treated
Tensile Strength, Yield 276 MPa

@Strain 0.200 %
40000 psi

@Strain 0.200 %
Heat Treated
Elongation at Break 30 %
30 %
Heat Treated
Component Elements Properties Metric English Comments
Aluminum, Al <= 0.050 %
<= 0.050 %
Carbon, C <= 0.15 %
<= 0.15 %
Chromium, Cr 12.5 %
12.5 %
Copper, Cu <= 0.50 %
<= 0.50 %
Iron, Fe >= 83.4 %
>= 83.4 %
As Remainder
Manganese, Mn <= 1.0 %
<= 1.0 %
Molybdenum, Mo <= 0.50 %
<= 0.50 %
Nickel, Ni <= 0.75 %
<= 0.75 %
Nitrogen, N <= 0.080 %
<= 0.080 %
Phosphorous, P <= 0.025 %
<= 0.025 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.015 %
<= 0.015 %
Tin, Sn <= 0.050 %
<= 0.050 %
Users viewing this material also viewed the following: