Tensile Strength, Ultimate 82.0 MPa
11900 psi
Ineos ABS Triax® 1315 GF ABS + Polyamide Blend (DAM)
Key Features:Contains FillerSuitable processing methods:Injection molding
Tensile Strength, Ultimate 82.0 MPa
11900 psi
DIN 53455; ASTM D638
Kolon Kopa® KN133 Nylon 6 Resin
KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c..
Tensile Strength, Ultimate 82.0 MPa
11900 psi
ASTM D638
Plenco 1530 Polyester, Briquette, Injection Molded
PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab..
Tensile Strength, Ultimate 82.0 MPa
11900 psi
5 mm/min
Arkema Group Rilsan® AZM 23 T6LD Nylon 12, 23% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA12,MHLR,16-050,GF23Rigid grade with glass fiber filler (23%) for injection molding. Available colors: black and natural. Reinforced light and heat stabilizing agent. Mold-rele..
Tensile Strength, Ultimate 82.0 MPa
11900 psi
ATSM D638
Ashley Polymers Ashlene® 265 PPO, 20% Glass Reinforced
A general purpose, 20% glass reinforced PPO resin for injection molding applications.Data provided by the manufacturer
Tensile Strength, Ultimate 82.0 MPa
11900 psi
AIM 52In/48Sn Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.
Tensile Strength, Ultimate 82.0 MPa
11900 psi
ASTM D638
A. Schulman ComAlloy Hiloy® 628 Nylon 6/6, Mineral Reinforced
Data provided by the manufacturer, ComAlloy International Company.30% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.