Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 855 MPa @Temperature -80.0 °C |
124000 psi @Temperature -112 °F |
EN min; EN 10002-5 |
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C.. |
|||
Tensile Strength, Ultimate | 855 MPa | 124000 psi | Typical |
Kinetics MIM K3 Heat Treat as Sintered K3 is a custom Mo-Fe alloy that provides improved fatigue properties over many other steel alloys while still maintaining good strength components, industrial or structural components and other appl.. |
|||
Tensile Strength, Ultimate | 855 MPa | 124000 psi | 4 in. Test Specimen |
Latrobe Lescalloy® 410Cb High Strength Stainless Steel LESCALLOY 17-4 VAC-ARC steel is a precipitation hardening martensitic stainless steel. A wide range of mechanical properties is available via simple aging within a 900-1150°F (482-621°C) tempe.. |
|||
Tensile Strength, Ultimate | 855 MPa @Temperature 540 °C |
124000 psi @Temperature 1000 °F |
|
Haynes 263® alloy, cold rolled sheet, solution treated and aged Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle.. |
|||
Tensile Strength, Ultimate | 855 MPa @Temperature 760 °C |
124000 psi @Temperature 1400 °F |
|
Haynes 718 alloy, cold rolled, solution-treated and aged sheet Cb and Ta content combined weight percentage of 5. Excellent high-temperature strength up to 650°C, good ductility, formability, and weldability. Very good welding characteristics. Applications i.. |
|||
Tensile Strength, Ultimate | 855 MPa | 124000 psi | |
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Annealed Round Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Annealed Round samples. Other property values are typical of INCONEL® alloy 725.Data provided.. |
|||
Tensile Strength, Ultimate | 855 MPa @Temperature 316 °C |
124000 psi @Temperature 600 °F |
H1150 |
Crucible Steel 15-5 Precipitation Hardening Stainless Steel Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is a V.. |
|||
Tensile Strength, Ultimate | 855 MPa @Temperature 316 °C |
124000 psi @Temperature 600 °F |
H1150 |
Crucible Steel 17Cr-4Ni Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a precipitation-hardening stainless steel which is capable of a high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is martensitic a.. |
|||
Tensile Strength, Ultimate | 855 MPa @Temperature 316 °C |
124000 psi @Temperature 600 °F |
H1150 |
Crucible Steel 17Cr-4Ni Super-X® Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a version of 17CR-4Ni which has been modified to substantially improve machinability and other properties. Patented 17Cr-4Ni Super-X meets industry specifications for 17Cr-4Ni. .. |
|||
Tensile Strength, Ultimate | 855 MPa @Thickness 22.2 mm |
124000 psi @Thickness 0.875 in |
Typical for Plate, Annealed |
AK Steel NITRONIC® 30 Austenitic Stainless Steel AK Steel NITRONIC 30 Stainless Steel offers significantly higher strength than Type 304 and potential for applications requiring good resistance to aqueous and atmospheric corrosion resistance combi.. |
|||
Tensile Strength, Ultimate | 855 MPa | 124000 psi | |
Haynes Multimet® alloy, 6.15 mm hot-rolled bar, 10% cold reduction Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductility, and i.. |