Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Latrobe Lescalloy® 410Cb High Strength Stainless Steel

Category Metal , Ferrous Metal , Stainless Steel
Manufacturer Latrobe Steel
Trade Name Lescalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Latrobe Lescalloy® 410Cb High Strength Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LESCALLOY 17-4 VAC-ARC steel is a precipitation hardening martensitic stainless steel. A wide range of mechanical properties is available via simple aging within a 900-1150°F (482-621°C) temperature range. Vacuum arc remelting provides low gas content, superior cleanliness and optimum transverse properties.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Specific Gravity 7.75 g/cc
7.75 g/cc
Density 7.75 g/cc
0.280 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 255
255
4 in. Test Specimen
255
255
5.25 in. Test Specimen
Tensile Strength, Ultimate 848 MPa
123000 psi
5.25 in. Test Specimen
855 MPa
124000 psi
4 in. Test Specimen
Tensile Strength, Yield 724 MPa

@Strain 0.200 %
105000 psi

@Strain 0.200 %
5.25 in. Test Specimen
731 MPa

@Strain 0.200 %
106000 psi

@Strain 0.200 %
4 in. Test Specimen
Elongation at Break 21 %
21 %
4 in. Test Specimen
22 %
22 %
5.25 in. Test Specimen
Reduction of Area 65 - 66 %
65 - 66 %
4 in. Test Specimen
66 %
66 %
5.25 in. Test Specimen
Modulus of Elasticity 200 GPa
29000 ksi
Machinability 50 - 55 %
50 - 55 %
Mild Steel
Charpy Impact 60.0 J
44.3 ft-lb
V-Notch; 5.25 in. Test Specimen
98.0 J
72.3 ft-lb
V-Notch; 4 in. Test Specimen
Thermal Properties Metric English Comments
CTE, linear 10.1 µm/m-°C

@Temperature 21.0 - 204 °C
5.61 µin/in-°F

@Temperature 69.8 - 399 °F
12.1 µm/m-°C

@Temperature 20.0 - 649 °C
6.72 µin/in-°F

@Temperature 68.0 - 1200 °F
Specific Heat Capacity 0.460 J/g-°C

@Temperature 0.000 - 100 °C
0.110 BTU/lb-°F

@Temperature 32.0 - 212 °F
Thermal Conductivity 25.0 W/m-K

@Temperature 100 °C
174 BTU-in/hr-ft²-°F

@Temperature 212 °F
Component Elements Properties Metric English Comments
Carbon, C 0.13 %
0.13 %
Chromium, Cr 11.6 %
11.6 %
Iron, Fe 86.79 %
86.79 %
Manganese, Mn 0.50 %
0.50 %
Nickel, Ni 0.60 %
0.60 %
Niobium, Nb (Columbium, Cb) 0.080 %
0.080 %
Silicon, Si 0.30 %
0.30 %
Users viewing this material also viewed the following: