Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 204 g | 204 g | ISO 6383-2 |
Iran Petrochemical (PCC) MF3313 High Density Polyethylene MF3313 is a high molecular weight high density polyethylene . Applications: extrusion, film, blown, bags, and density modifies.Information provided by Iran Petrochemical Commercial Co. |